News Center

How to ensure the balance of glue injection in each cavity of multi cavity mold hot runner?

Date:2026-11-14 Hits:6

Core principle: * * Prioritize geometric natural balance, then use mold flow simulation to predict, relying on independent temperature control, needle valve timing, machining accuracy, and process verification to provide a bottom line * * Meto Mold


###1. Channel layout: prioritize natural balance (the most stable)


Adopting an H-shaped, radially symmetrical arrangement, from the inlet of the splitter plate to each hot nozzle, the process, corner, and channel diameter are completely consistent;

When the number of cavities cannot be symmetrically equal, non natural equilibrium (compensating flow channel) should be achieved: the distal flow channel should be appropriately enlarged, the proximal flow should be limited, and the pressure drop difference should be compensated by the cross-sectional area of the flow channel. It is not enough to rely solely on later hard tuning processes to conceal the inherent imbalance.


> 

>Note: Even if the paths are of equal length, there is still a Beaumont effect (shear heat difference), and high cavity numbers and fiberglass materials will still be imbalanced.


###2. Pre simulation of flow modeling


Before cutting, perform Moldflow analysis to check the filling time, pressure, shear rate, and material temperature of each cavity, and adjust the diameter, angle, and hot nozzle position of the splitter plate flow channel in advance;

Objective: To control the filling time difference of each cavity within a very small range, not just based on the consistency of weight Meto Mold.


###3. Processing accuracy of splitter plate and hot nozzle


-The machining tolerance of the channel hole is strictly controlled, the inner wall is polished evenly, the roughness is consistent, and the difference in resistance is reduced;

-Smooth transition at corners to avoid dead corners, steps, and carbon deposits;

-The specifications of the hot nozzle and gate are uniform, and the throttling effect of the gate is consistent. The gate is an easily overlooked point of imbalance.


###4. Independent zone temperature control (the most commonly used fine-tuning method for hot runners)


**Each nozzle is independently temperature controlled (not a single temperature zone for the entire splitter plate):

Lower the temperature and increase the viscosity of the fast filled chamber to limit the flow; The slowly filled cavity heats up slightly, reducing the resistance of the melt;

⚠️  The adjustment range cannot be large, and design defects cannot be forcibly compensated for by temperature differences, as it is prone to burning, degradation, and carbon deposition.


###5. Needle valve hot runner: sequential valve opening (high-order solution)


When there is a large difference in the length of the multi chamber path, use a sequential valve gate: open the distal valve needle ahead of time and the proximal valve needle behind time to compensate for the time difference in material flow arrival; Suitable for products with 16 or more cavities, thin walls, and long processes; Open hot runner cannot achieve timing control Meto Mold.


###6. Synchronization of mold temperature, exhaust, and cooling


Each cavity has a symmetrical waterway and uniform mold temperature; Uniform exhaust positions, depths, and quantities for each chamber; If a certain chamber's exhaust is blocked, it will be directly manifested as slow filling of glue, lack of material, and misjudged as an imbalance in the hot runner.


###7. Mass production verification method (to determine whether it is flat or unbalanced)


1. Short shot test (holding pressure at 0): Check if the filling contour of each cavity is synchronized;

2. Weigh each cavity separately and calculate the weight deviation;

3. Optional cavity pressure sensor, check the alignment of pressure curves in each cavity;

4. Stable raw materials, drying, back pressure, and firing rate curves, and fluctuations in raw materials can also disrupt the balance.


###8. Avoiding pitfalls reminder


-Open hot runner balance difficulty>needle valve;

-Adding shear sensitive materials such as fiberglass and flame retardant significantly increases the difficulty of balancing;

-Don't simply rely on maintaining pressure to "flatten", as some cavities may experience excessive pressure and flash, while others may shrink.